材料名稱 Coating material |
化學成分(fēn)(%) Chemical composition |
塗層分(fēn)類 Coating classification |
塗層功能 Coating function |
塗層硬度(HV0.3) Coating hardness(HV0.3) |
噴塗方法 Spraying method |
塗層性能 Coating performance |
氧化鋁 Aluminium oxide |
Al2O3(〉99.3%) |
陶瓷 Ceramic |
絕緣、耐高溫 Insulation, high temperature resistant |
高(700-900) High (700-900) |
等離(lí)子噴塗 APS |
白(bái)色塗層,高熔點,耐熱,高絕緣性 White coating, high melting point, heatproof, high insulation |
氧化鋁钛AT3 Aluminium oxide- titanium oxide(AT3) |
Al2O3(97%)+TiO2(3%) |
陶瓷 Ceramic |
絕緣、耐磨 Insulation, abrasion resistant |
高(700-900) High (700-900) |
等離(lí)子噴塗 APS |
灰色塗層,耐磨、耐蝕、耐熱、絕緣 Grey coating, abrasion resistant, corrosion resistant, heatproof, insulation |
氧化鋁钛AT13 Aluminium oxide- titanium oxide(AT13) |
Al2O3(87%)+TiO2(13%) |
陶瓷 Ceramic |
硬面耐磨 Hard surface abrasion resistant |
高(800-1000) High (800-1000) |
等離(lí)子噴塗 APS |
黑色塗層,高耐磨性、耐腐蝕 Black coating, high abrasion resistance, corrosion resistance |
氧化鋁钛AT20 Aluminium oxide- titanium oxide(AT20) |
Al2O3(80%)+TiO2(20%) |
陶瓷 Ceramic |
硬面耐磨 Hard surface abrasion resistant |
高(750-950) High (750-950) |
等離(lí)子噴塗 APS |
黑色塗層,高耐磨性,塗層緻密 Black coating, high abrasion resistance, compact coating |
氧化鋁钛AT40 Aluminium oxide- titanium oxide(AT40) |
Al2O3(60%)+TiO2(40%) |
陶瓷 Ceramic |
硬面纖維耐磨 Hard surface fiber abrasion resistant |
高(650-850) High (650-850) |
等離(lí)子噴塗 APS |
黑色塗層,結合強度好,塗層緻密,耐磨,摩擦系數低 Black coating, good bonding strength, compact coating, abrasion resistant, low friction coefficient |
氧化鉻 Chromic oxide |
Cr2O3 |
陶瓷 Ceramic |
硬面纖維耐磨 Hard surface fiber abrasion resistant |
高(950-1300) High (950-1300) |
等離(lí)子噴塗 APS |
深墨綠色塗層,高硬度、高耐磨性、耐腐蝕、耐沖刷、摩擦系數低 Deep green coating, high hardness, high abrasion resistance, corrosion resistant, washout resistant, low friction coefficient |
氧化锆 Zirconium oxide |
ZrO2+Y2O3(6-8%) |
陶瓷 Ceramic |
高溫熱障 High temperature thermal barrier |
高(500-700) High (500-700) |
等離(lí)子噴塗 APS |
導熱系數低,耐燒蝕、耐熱震性能好 Low heat conductivity coefficient, good ablation resistance and thermal shock resistance |
氧化钇 Yttrium oxide |
Y2O3 |
陶瓷 Ceramic |
耐高溫 High temperature resistant |
高(1500-2000) High (1500-2000) |
等離(lí)子噴塗 APS |
耐等離(lí)子體(tǐ)腐蝕,應用于半導體(tǐ)矽片蝕刻 Plasma corrosion resistance used in semiconductor silicon chip etching |
莫來石 Mullite |
Al2O3+SiO2 |
陶瓷 Ceramic |
耐高溫 High temperature resistant |
高(700-900) High (700-900) |
等離(lí)子噴塗 APS |
耐高溫、耐熱震性能好 Good high temperature resistance and thermal shock resistance |
鋁鎂尖晶石 Alumina-magnesia spinel |
Al2O3+MgO |
陶瓷 Ceramic |
耐磨、耐堿性腐蝕 Abrasion resistant, alkaline corrosion resistant |
高(700-900) High (700-900) |
等離(lí)子噴塗 APS |
耐磨、耐堿性腐蝕 Abrasion resistant, alkaline corrosion resistant |
亞氧化钛 Titanium black |
Ti4O7 |
陶瓷 Ceramic |
導電(diàn) Conduct electricity |
高(500-700) High (500-700) |
等離(lí)子噴塗 APS |
具有類金屬的導電(diàn)性,耐腐蝕,優異的電(diàn)化學性能 Has metal-like electrical conductivity, corrosion resistant, excellent electrochemical property |
鎳包石墨 Nickel-coated graphite |
Ni(50%)+C(50%) |
複合塗層 Composite coating |
自潤滑 Self-lubricating |
軟 Soft |
等離(lí)子噴塗 APS |
優異的自潤滑性能 Excellent self-lubricating property |
鋁矽聚苯脂 Aluminum silicon polyphenyl ester |
AlSi(60%)+polyester(40%) |
複合塗層 Composite coating |
可磨耗封嚴塗層 Abradable sealing coating |
中(zhōng) Medium |
等離(lí)子噴塗 APS |
耐高溫,耐沖蝕,硬度适中(zhōng),可磨耗,間隙适應 High temperature resistant, erosion resistant, moderate hardness, abradable |
鎳基合金 Nickel base alloy |
NiCrBSi |
合金 Alloy |
耐磨、耐腐蝕 abrasion resistant, corrosion resistant |
高(500-700) High (500-700) |
等離(lí)子噴塗 APS |
耐磨性好,耐腐蝕,耐沖擊 Good abrasion resistance, corrosion resistant, impact resistant |
钴基碳化鎢 Cobalt base tungsten carbide |
WC(88%)+Co(12%) |
金屬陶瓷 Metal ceramic |
高耐磨、耐沖擊 High abrasion resistant, impact resistant |
高(1000-1400) High (1000-1400) |
超音速火(huǒ)焰 HVOF |
硬度高,韌性好,耐高壓沖擊磨損 high hardness, good toughness, High pressure impact abrasion resistant |
钴鉻碳化鎢 Cobalt chromium tungsten carbide |
WC(86%)+Co(10%)+Cr(4%) |
金屬陶瓷 Metal ceramic |
高耐磨、耐沖擊 High abrasion resistant, impact resistant |
高(1000-1400) High (1000-1400) |
超音速火(huǒ)焰 HVOF |
硬度高,韌性好,耐高壓沖擊磨損,耐腐蝕 high hardness, good toughness, High pressure impact abrasion resistant, corrosion resistant |
鎳鉻碳化鉻 Nickel chromium chromium carbide |
NiCr(25%)+Cr2C3(75%) |
金屬陶瓷 Metal ceramic |
高耐磨、耐沖擊 High abrasion resistant, impact resistant |
高(900-1200) High (900-1200) |
超音速火(huǒ)焰 HVOF |
硬度高,耐高溫腐蝕,耐沖蝕 High hardness, high temperature corrosion resistant, erosion resistant |
銅 Copper |
Cu |
金屬 Metal |
導電(diàn) Conduct electricity |
軟 Soft |
等離(lí)子噴塗 APS |
導電(diàn)性能好,塗層性能穩定 Good conductive performance, stable coating performance |
钼 Molybdenum |
Mo |
金屬 Metal |
高溫耐磨 High temperature abrasion resistant |
高(500-700) High (500-700) |
等離(lí)子噴塗 APS |
耐高溫,塗層具有微孔儲油功能,用于邊界摩擦 High temperature resistant, coating has the function of microporous oil storage, used in boundary friction |
鋁 Aluminum |
Al |
金屬 Metal |
耐腐蝕 corrosion resistant |
HB60-150 |
等離(lí)子噴塗 APS |
耐腐蝕性能好,光反射面塗層 Good corrosion resistance, light reflective surface coating |
鎳 Nickel |
Ni |
金屬 Metal |
耐腐蝕 corrosion resistant |
HV200-300 |
等離(lí)子噴塗 APS |
耐腐蝕,耐高溫氧化 Corrosion resistance, high temperature oxidation resistance |